Architecture Paint

ENERGY SAVER(WATER-BASED) Water-based heat reflective insulation paint

usage
Roofs and walls or inner walls and ceilings of factories, warehouses, houses, buildings, etc.
Other places where insulation is required

This paint is a water-based heat reflective insulation paint made by using special acrylic emulsion resin and ceramic material with excellent weather resistance. It not only reflects heat rays from sunlight during painting but also prevents the heat from being transferred to the inside, thereby showing an excellent insulation effect. It has excellent adhesion with the existing coating surface, weather resistance and chemical resistance. It is a premium water-based eco-friendly product that can remarkably reduce cooling/heating costs by making it difficult for the outside heat to be transferred to the inside and for the inside heat to come out at the same time due to its low thermal conductivity.

specification

Paint type
Acrylic emulsion water-based / Top coat
Drying time
Drying time
Category 5℃ 20℃ 30℃
Set-to-touch 1 hour 30 minutes 20 minutes
Dry-through 6 hours 3 hours 2 hours
Time required for re-coating (min.) 8 hours 4 hours 3 hours
Thinner
Less than 10~15% tap water, if necessary
Coating Method
Brush, roller, spray coating.
Specific gravity
Approx. 0.7(Based on white color)
Solid volume ratio
Approx. 65.4 %
Theoretical Coverage
1.3 ㎡/ℓ
Thickness of dried film
500㎛ (4~5times)
Re-coating interval
20℃, sufficient ventilation for a minimum of 5 hours
Color
White
Gloss
Matte
Storage and preservation
12 months (well-ventilated dry, cold and dark location, room temperature 5℃~30℃, humidity less than 80%)

PRODUCT PROPERTIES (PHYSICAL PROPERTY DATA)

Heat reflection insulation performance
By applying special ceramic pigments, it has excellent infrared reflectance and low thermal conductivity.
Dense film composition
By forming a dense film, durability including adhesion, weather resistance, and chemical resistance is excellent.

how to use

Surface treatment
1. The material should be sufficiently cured (cured more than 30 days at 20℃)
2. Laitance, dust, oil and other contaminants on the surface must be completely removed.
3. The proper pH of the material must be less than 9, and the percentage of moisture content must be less than 6%.
4. The gaps and grooves on the surface must be filled with Elastic putty, and surface adjustment should be made before coating.
Coating method
1. Primer
① After surface treatment, if necessary, dilute the water-based epoxy undercoat with water up to 10% and apply once with a roller or brush to get a dry film thickness of 20㎛.
② For areas where the absorption of the surface is severe, apply once more coating.
2. Top coat
① After at least 8 hours at 20℃ following undercoating, apply this paint 4~5 times with a brush, roller or spray to get a dry film thickness of 500㎛.
② At this time, undiluted paint is recommended, but if necessary, it can be diluted to less than 5% with tap water for coating.