Architecture Paint
YEGREENA STONE EVER Primer/Intermediate coating
- usage
- Coatings for interior, exterior walls of buildings such as concrete and cement mortar
Apartments, buildings and multi-family housing specialized areas (ground level, pilotties, canopies), etc.
YEGREENA STONE EVER primer/intermediate coating is a paint that manufactured by using acrylic copolymer binder. It is a pattern type coat to make embossing patterns. It increases the adhesion between primer and top coat, enhances the sense of volume of real stone and realizes more realistic stone pattern. It is a medium embossing patterning material which has strong adhesion, air permeability, weatherability and various pattern formation. It has excellent compatibility with other finish materials.
specification
- Paint type
- Waterborne acrylic emulsion
- Drying time
-
Drying time Category 20℃ Time required for re-coating (min.) 24 hours Over-coat 24 hours - Thinner
- Tap water(dilution rate: less than 5%)
- Coating Method
- Spray coating (Bone tile gun)
- Specific gravity
- Approx. 1.4~1.6
- Color
- Ordered colors
- Theoretical Coverage
- 1.0~1.4 ㎏/㎡ (It can be changed depedning on the color and petterns.)
- Storage and preservation
- 12 months (well-ventilated dry, cold and dark location, room temperature 5℃~30℃, humidity less than 80%)
PRODUCT PROPERTIES (PHYSICAL PROPERTY DATA)
- Workability
- The range of choice of consumers is broad as colors and pattern sizes are diverse.
- Environmental impact
- It is an eco-friendly product having almost no VOC and odor.
how to use
- Surface treatment
- 1. The material should be sufficiently cured (cured more than 30 days at 20℃)
2. Laitance, dust, oil and other contaminants on the surface must be completely removed.
3. The proper pH of the material must be less than 9, and the percentage of moisture content must be less than 6%.
4. The gaps and grooves on the surface must be filled with exterior water-based putty, and surface adjustment should be made before coating. - Coating method
- 1. Once you start work, you should continue to execute the work.
2. Proceed in the direction of the corner from the edge of the wall.
3. Use a dedicated gun, and it is suitable that depending on the pattern, the fluid tip is 3 - 8㎜ and the air pressure is 3 - 5kg f/㎠.
4. Depending on the spraying method, there may be differences in color and pattern. Thus, start application in earnest after trial coating.
5. Do not let seams occur when you stop working inevitably.
6. It must be protected from other external damage such as pollutants, shock, water, etc. until it is completely dry.
7. For undercoating, use the designated primer(YEGREENA STONE EVER PRIMER).