Heavy Duty Coating

SPEEDPOXY 100 Fast-drying epoxy anti-corrosive primer

usage
Anti-corrosive primer for steel structures requiring long-term anti-corrosion

This paint is a two-component anti-corrosive paint made mainly of active oxidized steel and an excellent anti-corrosive pigment based on epoxy resin. This paint dries very fast, has excellent adhesion to steel surfaces and forms a hard dry film at the same time. It is excellent in anti-corrosive properties, water resistance and oil resistance and is suitable as an anti-corrosive paint for various steel structures. It is a fast-drying epoxy anti-corrosive primer that has the advantage of being able to complete the top coat within one day due to the fast drying speed.

specification

Paint type
Epoxy / Anti-corossive primer (Two-Component)
Drying time
Drying time
Category 5℃ 20℃ 30℃
Set-to-touch 40 minutes 20 minutes 10 minutes
Dry-hard 5 hours 3 hours 1 hour
Over-coat (Min.) 7 hours 4 hours 2 hours
Over-coat (Max.) 1 month 15 days 7 days
Maturation time 30 minutes 20 minutes 10 minutes
Pot life 8 hours 6 hours 4 hours
Thinner
DR-100
Dilution ratio
▷Brush, roller coating: less than 15% ▷Airless, spray coating: less than 10%
Specific gravity
Approx 1.3(Based on reddish brown)
Theoretical Coverage
10 ㎡/ℓ (1time - 50㎛)
Solid volume ratio
Approx. 50±1%
Color
Reddish brown, other colors
Thickness of dried film
50㎛
Mixing ratio
Base(A)/Hardener(B)=3/1 (Volume ratio)
Flash point
At least 7℃
Gloss
Matte
Shelf life
12 months (Dry, cool, and dark place with good ventilation)

PRODUCT PROPERTIES (PHYSICAL PROPERTY DATA)

Quick-drying speed
The drying speed is fast among epoxy type anti-corrosive undercoats.
Excellent film property
Water resistance, oil resistance, and anti-corrosive properties are excellent, and it can be applied to the inside of crude oil or water tanks.

how to use

Surface treatment
1. Completely remove oil, moisture, sand, dust, and other foreign matter from the surface to be coated.
The degree of surface treatment to obtain an excellent steel protection effect should be at least SSPC-SP 10
or Sa2.5 (near white metal blast cleaning).The surface roughness should not exceed 75 ㎛.
2. For steel, apply immediately after surface treatment.
3. After primer coating, clean up the welded areas (blackened and rusted areas) with a disc sander.
Then, touch up with this paint and continue coating.
Coating method
1. Coating can be done by either brush, roller, air or airless spray coating.
2. Airless spray coating:
- Tip diameter : 0.015"~0.021"
- Injection pressure : More than 2500 P.S.I(176㎏/㎠)
- Store the coating equipment after cleaning with an exclusive thinner immediately after use.
Preceding and follow-up coating
1. Follow-up coating : Epoxy resin, urethane resin, PVDF paint are sutaible.
Remarks
1. Sufficient performance after last coating is achieved after drying for 7 days at 20℃.
2. For coating areas exposed to the outside, yellowing and chalking may occur in a short period of time due to
the effect of sunlight. Upon coating for areas exposed to the outside, be sure to apply top coat.