Heavy Duty Coating

DHDC-0690ZP-HB Epoxy anti-corrosive primer, high build

usage
Anti-corrosive primer for steel structures and zinc plated steel surfaces requiring long-term anti-corrosion

This paint is an anti-corrosive paint made by using zinc phosphate, an excellent anti-corrosive pigment, and epoxy-modified polyamide resin. This paint has an excellent anti-corrosive effect when applied to steel structures and is widely used as an primer of general epoxy paints. It can be used as an primer for the surface of hot dip (electro) galvanized coating.

specification

Paint type
Epoxy modified polyamide / Anti-corossive primer / High build (Two-Component)
Drying time
Drying time
Category 5℃ 20℃ 30℃
Set-to-touch 2 hours 1 hour 40 minutes
Dry-hard 20 hours 10 hours 8 hours
Over-coat (Min.) 32 hours 15 hours 12 hours
Over-coat (Max.) 4 months 3 months 2 months
Maturation time 1 hour 30 minutes 20 minutes
Pot life 16 hours 12 hours 8 hours
Thinner
DR-100
Dilution ratio
▷Brush, roller coating: less than 15% ▷Airless, spray coating: less than 10%
Specific gravity
Approx. 1.3(Based on reddish brown)
Theoretical Coverage
5.2 ㎡/ℓ (1time - 100㎛)
Solid volume ratio
Approx. 52±1%
Color
Gray, other colors
Thickness of dried film
100㎛
Mixing ratio
Base(A)/Hardener(B)=3/1 (Volume ratio)
Flash point
At least 7℃
Gloss
Matte
Shelf life
12 months (Dry, cool, and dark place with good ventilation)

PRODUCT PROPERTIES (PHYSICAL PROPERTY DATA)

Excellent film property
Water resistance, oil resistance, and anti-corrosive properties are excellent, and it can be applied to the inside of crude oil or water tanks.
Primer of galvanized surfaces
Applicable for the primer of hot-dip (electro) galvanized surfaces

how to use

Surface treatment
1. Completely remove oil, moisture, sand, dust, and other foreign matter from the surface to be coated.
The degree of surface treatment to obtain an excellent steel protection effect should be at least SSPC-SP 10
or Sa2.5 (near white metal blast cleaning).The surface roughness should not exceed 75 ㎛.
2. For steel, apply immediately after surface treatment.
3. After primer coating, clean up the welded areas (blackened and rusted areas) with a disc sander.
Then, touch up with this paint and continue coating.
Coating method
1. Although coating can be done by either brush or airless spraying, airless spray coating is best.
2. Airless spray coating:
- Tip diameter : 0.019"~0.025"
- Injection pressure : More than 2500 P.S.I(176㎏/㎠)
- Store the coating equipment after cleaning with an exclusive thinner immediately after use.
Preceding and follow-up coating
1. Follow-up coating : Epoxy resin, urethane resin, PVDF paint are sutaible.
Remarks
1. Sufficient performance after last coating is achieved after drying for 7 days at 20℃.
2. For coating areas exposed to the outside, yellowing and chalking may occur in a short period of time due to
the effect of sunlight. Upon coating for areas exposed to the outside, be sure to apply top coat.