Heavy Duty Coating

DHDC-0696HB Epoxy anti-corrosive primer, high build

usage
Steel structures requiring long-term anti-corrosion and places requiring water resistance and oil resistance

This paint is a high build epoxy primer that contains the best anti-corrosive pigment in addition to epoxy polyamide resin. It is a high build epoxy paint that can be applied as the dry film of up to 100㎛ in one coat. Unlike conventional anti-corrosive primers, it has the advantage of shortening the work process and is excellent in adhesion, water resistance, salt water resistance, oil resistance, and solvent resistance.

specification

Paint type
Epoxy modified polyamide / Anti-corossive primer /High build (Two-Component)
Drying time
Drying time
Category 5℃ 20℃ 30℃
Set-to-touch 2 hours 1 hour 40 minutes
Dry-hard 24 hours 10 hours 8 hours
Over-coat (Min.) 32 hours 15 hours 12 hours
Over-coat (Max.) 4 months 3 months 2 months
Maturation time 1 hour 30 minutes 20 minutes
Pot life 16 hours 12 hours 8 hours
Thinner
DR-100
Dilution ratio
▷Brush, roller coating: less than 15% ▷Airless, spray coating: less than 10%
Specific gravity
Approx. 1.4(Based on reddish brown)
Theoretical Coverage
6 ㎡/ℓ (1time - 100㎛)
Solid volume ratio
Approx. 60±1%
Color
Reddish brown, gray, other colors
Thickness of dried film
75~100㎛
Mixing ratio
Base(A)/Hardener(B)=6/1 (Weight ratio)
Flash point
At least 7℃
Gloss
Matte
Shelf life
12 months (Dry, cool, and dark place with good ventilation)

PRODUCT PROPERTIES (PHYSICAL PROPERTY DATA)

Reduce process
A high-build long-term anti-corrosive primer with excellent adhesion to steel surfaces, it can reduce the painting process.
Excellent film property
Water resistance, oil resistance, and anti-corrosive properties are excellent, and it can be applied to the inside of crude oil or water tanks.

how to use

Surface treatment
1. Completely remove oil, moisture, sand, dust, and other foreign matter from the surface to be coated.
The degree of surface treatment to obtain an excellent steel protection effect should be at least SSPC-SP 10
or Sa2.5 (near white metal blast cleaning).The surface roughness should not exceed 75 ㎛.
2. For steel, apply immediately after surface treatment.
3. After primer coating, clean up the welded areas (blackened and rusted areas) with a disc sander.
Then, touch up with this paint and continue coating.
Coating method
1. Although coating can be done by either brush or airless spraying, airless spray coating is best.
2. Airless spray coating:
- Tip diameter : 0.019"~0.025"
- Injection pressure : More than 3000 P.S.I(210㎏/㎠)
- Store the coating equipment after cleaning with an exclusive thinner immediately after use.
Preceding and follow-up coating
1. Follow-up coating : Epoxy resin, urethane resin, PVDF paint are sutaible.
Remarks
1. Sufficient performance after last coating is achieved after drying for 7 days at 20℃.
2. For coating areas exposed to the outside, yellowing and chalking may occur in a short period of time due to
the effect of sunlight. Upon coating for areas exposed to the outside, be sure to apply top coat.