Heavy Duty Coating
REL-PON 28 Epoxy amine-adduct primer, high build
- usage
- Steel tank interior primer (oil and solvent tanks, etc.)
- data
- REL-PON 28.pdf
This paint is a high build epoxy primer made by using epoxy resin and the best anti-corrosive pigment. It is a coating material for tank lining designed as an primer for oil and solvent tanks due to its excellent adhesion, water resistance, salt water resistance and solvent resistance.
specification
- Paint type
- Epoxy / Anti-corrosive primer / High build (Two-Component)
- Drying time
-
Drying time Category 5℃ 20℃ 30℃ Set-to-touch 2 hours 1 hour 40 minutes Dry-hard 24 hours 18 hours 16 hours Over-coat (Min.) 32 hours 24 hours 20 hours Over-coat (Max.) 2 months 1 month 15 days Maturation time 1 hour 30 minutes 20 minutes Pot life 16 hours 12 hours 8 hours - Thinner
- DR-100
- Dilution ratio
- ▷Brush, roller, spray coating: less than 10%
- Specific gravity
- Approx. 1.4
- Theoretical Coverage
- 5.5 ㎡/ℓ (1time - 100㎛)
- Solid volume ratio
- Approx. 55±1%
- Color
- Gray, reddish brown
- Thickness of dried film
- 100㎛
- Mixing ratio
- Base(A)/Hardener(B)=6/1 (Weight ratio)
- Flash point
- At least 7℃
- Gloss
- Matte
- Shelf life
- 12 months (Dry, cool, and dark place with good ventilation)
PRODUCT PROPERTIES (PHYSICAL PROPERTY DATA)
- Primer for tanks
- A two-componet epoxy amine-adduct primer for petroleum solvent for metal tanks (high-build type)
- Excellent film property
- Adhesion, oil resistance, salt water resistance, and solvent resistance are excellent.
how to use
- Surface treatment
- 1. Completely remove oil, moisture, sand, dust, and other foreign matter from the surface to be coated.
The degree of surface treatment to obtain an excellent steel protection effect should be at least SSPC-SP 10
or Sa2.5 (near white metal blast cleaning).The surface roughness should not exceed 75 ㎛.
2. For steel, apply immediately after surface treatment.
3. After primer coating, clean up the welded areas (blackened and rusted areas) with a disc sander.
Then, touch up with this paint and continue coating. - Coating method
- 1. Although coating can be done by either brush or airless spraying, airless spray coating is best.
2. Airless spray coating:
- Tip diameter : 0.019"~0.025"
- Injection pressure : More than 3000 P.S.I(210㎏/㎠)
- Store the coating equipment after cleaning with an exclusive thinner immediately after use. - Preceding and follow-up coating
- 1. Follow-up coating : Epoxy resin paint(REL-PON 29), urethane resin, PVDF paint
- Remarks
- 1. Sufficient performance after last coating is achieved after drying for 7 days at 20℃.
2. For coating areas exposed to the outside, yellowing and chalking may occur in a short period of time due to
the effect of sunlight. Upon coating for areas exposed to the outside, be sure to apply top coat.